Appendix E 1.6 Checking Adhesion

A field check should be made by lifting an aggregate particle from the binder about one minute after spreading or dropping into freshly sprayed binder. The aggregate should retain a coating of binder as it is removed from the pavement. Little or no adhering binder can indicate a need to vary procedures (e.g. extended rolling) to ensure adequate adhesion.